Font Size: a A A

The use of superabsorbent polymer in standard and pervious concrete

Posted on:2012-09-02Degree:M.SType:Thesis
University:University of Missouri - Kansas CityCandidate:Farney, Christopher JohnFull Text:PDF
GTID:2452390011955760Subject:Engineering
Abstract/Summary:
The use of internal curing and specifically the use of super absorbent polymers has recently become an important topic in concrete research. Internal curing has been shown to reduce autogenous shrinkage in concrete mixtures, especially in high-strength mixtures where the water to cement ratio is low. Super absorbent polymer has not been studied in regards to its effect on pervious concrete. This research was conducted to examine the effectiveness of a commercially available super absorbent polymer in both standard and pervious concrete.;The testing was initially conducted on mortar mixtures, followed by standard and high-strength concrete mixtures, and finally pervious concrete mixtures. Several tests were conducted including compressive strength, autogenous and total shrinkage, restrained shrinkage, moisture loss, abrasion, as well as others.;The results followed similar trends as much of the previous research conducted on standard and high-strength mixtures containing super absorbent polymer. The pervious concrete containing super absorbent polymer showed an improvement in compressive strength, abrasion resistance, moisture loss, and total shrinkage compared to a control pervious mixture. If long term testing shows an improvement in the durability of pervious concrete containing super absorbent polymer, the applications for pervious concrete could be significantly increased.
Keywords/Search Tags:Absorbent polymer, Pervious concrete, Internal curing
Related items