Font Size:
a
A
A
Keyword [Nickel based superalloy]
Result: 101 - 120 | Page: 6 of 10
101.
Research On Electrochemical Machining Of Holes In Nickel-based Superalloy
102.
The Effect Of Transient Liquid Phase Bonding On Microstructure And Mechanical Properties Of Mar-M247 Nickel-based Superalloys Joints
103.
Experimental Study Of Processing Property Of Single Crystal Material In Micro-grinding
104.
Study On Cutting Deformation Of High Speed Cutting GH4169
105.
Analysis And Study On The Characteristics Of Short Arc Machining Of Nickel Based Superalloy
106.
Physical Simulation And Process Parameter Optimization Of Nickel-based Superalloy Machining
107.
Preparation And Properties Of Nickel-based Superalloys
108.
Study On High Temperature Oxidation Performance Of Hot Dip-plated Si Modified Aluminide Coating Under Different Conditions
109.
Study On Fabrication And Properties Of Ceramic Cutting Tools For High Speed Machining Nickel-based Superalloys
110.
Fundamental Research On The Ultra-high Speed Grinding Of Nickel-based Superalloy With CFRP Wheels
111.
Study On The Preparation And Oxidation Properties For The NiAl And RE Zr-doped NiAl Coating On Nickel-based Superalloy
112.
A Study On Surface Integrity Of Nickel Based Superalloy Inconel 718 Under Robotic Belt Grinding
113.
Multi-scale Coupling Numerical Simulation Of Directional Solidification Process Of Aeronautical Nickel-based Superalloy Blades
114.
Analysis On The Relationship Between Oxidation Kinetics And Oxide Film Structure Evolution Of The Nickel-based Superalloy
115.
Research On Process And Mechanism Of Diffusion Bonding DD3 Nickel-based Superalloy To Ti
3
AlC
2
Ceramic
116.
Microstructure And Mechanical Properties Of Cast Nickel-based Superalloy With High Tungsten Content Using For High-temperature Dies
117.
Mesoscopic Plastic Deformation Mechanism Of GH4169 Nickel-based Superalloy Thin Sheet
118.
Multi-scale Coupling Numerical Simulation Of Directional Solidification Process Of Aeronautical Nickel-Based Superalloy Blades
119.
Mechanism Of Dendrite Growth For Laser Additive Manufacturing Of Nickel-base Superalloy
120.
Research On Microstructure Simulation Of Hot Deformation Of GH4698 Nickel-based Superalloy
<<First
<Prev
Next>
Last>>
Jump to